Solutions
Horse Construction offers full range of structural strengthening materials with technical supports, documentation supports, products supports, project supports.
How To Reinforce Cracks In Cast-in-situ Concrete Floor Slab
How to reinforce the cracks in the cast-in-place concrete floor?
Today, I will talk about the crack grouting reinforcement method, which is one of the commonly used methods for the reinforcement of floor cracks. It is mainly aimed at early shrinkage cracks and is unlikely to continue to develop due to environmental impact. This method is more economical. After repairing, it is necessary to observe the cracks for one month to monitor the reinforcement effect.
When it comes to cracks, there are three main categories:
(1) Penetrating cracks> 0.5mm will cause corrosion of steel bars and affect the function of use. Automatic low-pressure grouting epoxy resin glue is used;
(2) Non-penetrating cracks with a width> 0.3mm will cause corrosion of steel bars and affect the durable bearing capacity of the structure. ECM water emulsion epoxy mortar or joint sealant is used for sealing treatment;
(3) Non-penetrating cracks with a width of ≤0.3mm have no harmful effect on the structural bearing capacity and durability, so it is not necessary to deal with it.
The standard construction process of HORSE grouting glue
First, remove the stucco layer within 10cm on both sides of the crack
According to the design requirements, slotting along the crack direction, grinding and trimming and cleaning up
Install the glue nozzle, the distance is about 10~30cm
Use HORSE sealant to seal cracks
After the sealing glue is solidified, start venting and pressure test. If there is any leakage, the glue injection nozzle should be repaired or re-embedded in time
Configure the HORSE joint sealant according to the specified ratio, and mix evenly without bubbles
Use the glue injection device to suck in the configured HORSE crack repair glue, and inject it from the glue nozzle. When glue overflows from the next glue nozzle, close the current glue nozzle and inject glue in sequence. The glue injection sequence should follow from low to high, and from side to side
After the glue has initially set, remove the glue injection device and the glue nozzle, and use the HORSE sealant to smooth it out
After the glue is cured for 7 days, carry out quality inspection
You can find anything here you are in need of, have a trust trying on these products, you will find the big difference after that.
Good thixotropy carbon fiber leveling adhesive for concrete surface repairing
High strength crack sealing repairing adhesive for the fracture surface of concrete crack
Very strong penetration and low viscosity epoxy crack injection adhesive for repairing concrete crack